Products

HIGH QUALITY CHINA MANUFACTURER SUP9 STEEL LEAF SPRING FOR TRAILER 2728
HIGH QUALITY CHINA MANUFACTURER SUP9 STEEL LEAF SPRING FOR TRAILER 2728

HIGH QUALITY CHINA MANUFACTURER SUP9 STEEL LEAF SPRING FOR TRAILER 2728

Short Description:

 

Part NO. TRA-2728 JC NO. JCBHZB0099
Spec. 76*20(mm) Model Hutchens Trailer
Material SUP9/55Cr3/SAE5160H MOQ 50 SETS
Port Shanghai/Xiamen/Ningbo Payment T/T,L/C,D/P
Lead Time 20-30 days Warranty 12 months
Description

This spring assy are widely used in American for trailer .

Spring Measurements Specs

Totally 3 blades , 3pcs middle pads , End to End Measurement 1124 mm (Free Length Measurement), A side Free Arch Measurement 97mm,Tolerance range ±3mm ,B side Free Arch Measurement 89mm,Tolerance range ±3mm, Middle straight 203mm .

All datas are obtained by measuring the new produce product .

HIGH QUALITY CHINA MANUFACTURER SUP9 STEEL LEAF SPRING FOR TRAILER 2728

NO.Leaf

W&T(mm)

Length(mm)

Per Weight(kg)

Assy Weight(kg)

1

76*20

578+546

12.35

26

2

76*20

383+383

8.28

3

76*20

235+235

4.84

TRA2728 Leaf Spring Detail Photos

1HIGH QUALITY CHINA MANUFACTURER SUP9 STEEL LEAF SPRING FOR TRAILER 2728
HIGH QUALITY CHINA MANUFACTURER SUP9 STEEL LEAF SPRING FOR TRAILER 2728
Key Points Keep The High Quality
1) Raw matrail .
Thickness less than 20mm. we choose SUP9/55Cr3/SAE5160H as the product material
Thickness from 20-30mm. wE choose SUP11A/50CrVA
Thickness more than 30mm. We choose 51CrV4 as the raw material
Thickness more than 50mm. We choose 52CrMoV4 as the raw material
2) Quchenging Process
We strickly controled the steel temeprure around 800 degree.
we swing the spring in the qenching oil among 10 seconds according to the spring thickness.
3)Shot Peening.
Each assmembing spring set under stress peening .
Fatigue test can reach over 150000 cycus
4) Painting
Each leaf under cataphoresis painting.
Salt spray testing reach 500hours
Production Process

1.Material Cutting

4.Edge Cutting

7.Stress PeeningCutting

2.Punching

5.Quenching

8.Assembling

3.Eye Rolling

6.Tempering

9.Painting

FAQ

Q1: What type of leaf spring could you produce ?

A: We can produce most kinds of springs in the market. especially on the parabolic springs.

Q2: What material could you supply for leaf spring?

A: Our material grade should be SUP9/SUP9A /SUP11A/51CrV4 /52CrMoV4/ even 55Cr3 and  SAE5160H as well .

Q3: How long will be your delivery time?

A: 20-40days. If material stock enough around 20days. if not,would be 40days

Q4: What payment terms are acceptable?

A: TT and LC at sight

Q5: What is the packing?

A: No fumigation wooden pallet . we also can pack according to whatever you request if reasonable.

Q6:How about the surface finishing ?

A : electrophoresis coating (black,red,gray,or as customer’s requests )

Send us a Message

Request a Quote

We would love to hear from you! Please fill out this form and we will get in touch with you shortly.